Read an experimental study of cure depth and adhesion, then a reanalysis of what the measurements can identify. Both distinguish the tested conditions from conclusions that would require further evidence.

Publications in this reading route

  1. Light Intensity versus Energy Dose in Vat Photopolymerization: Experimental Effects on Cure Depth and Adhesion
    View description

    Zenodo description

    Experimental study of a fixed transparent PEEK-like photopolymer formulation in a 405 nm LCD printer, comparing cure depth and qualitative adhesion under approximately matched radiant exposures. Three reported irradiances, four exposure times per irradiance and three specimens per condition provide 36 observations. Positive cure-depth data are summarized by a Jacobs working curve and tested for lack of fit against replicate pure error. The pooled fit gives apparent Dp = 67.06 µm and Ec = 16.57 mJ/cm² (R² = 0.986), with statistically detectable lack of fit. Adding irradiance category did not significantly improve the descriptive regression. The findings are restricted to the tested formulation and conditions and do not establish universal reciprocity.

    Version 1. English and Spanish PDFs and the CSV containing the 36 measurements are deposited together.

  2. What a Curing Curve Can Identify
    View description

    Zenodo description

    Interpreting resin response without confounding it with test effects

    A curing working curve, referred to here as CRT, relates radiant exposure to the resulting thickness of cured resin. Its usefulness depends on whether the light assigned to each sample and the measured thickness represent what occurred during the test. An excessively thin resin layer, an irradiance reading taken at a different position, or excessive micrometer tightening can alter the curve and, with it, the parameters used to interpret the material.

    This study reanalyses 36 existing observations grouped into 12 exposure conditions. It aims to explain which conclusions the data support and which depend on the chosen model or on measurement assumptions. Two different optical models describe the nine conditions with measurable curing in very similar ways. A calculated curve lying close to the data is therefore insufficient to identify the physical mechanism that produced them.

    The smallest maximum discrepancy from a Jacobs straight line is 7.938 µm. Curvature has a positive sign in all three blocks, whereas a fixed liquid-height cap applied to Jacobs gives a non-positive sign: that cap alone cannot explain the observed shape. The error scenarios delimit compatibility without measuring deformation or correcting the data.

    A frame retained a nominal resin height of 2 mm for all 36 samples. This preparation provides a substantial margin above the largest recorded cured thickness of 162 µm. It does not, by itself, demonstrate the absence of oxygen inhibition. Applying a CRT to printing requires joint consideration of liquid height, oxygen access, exposure position, source spectrum and measurement procedure.

Application documentation at 3Dresyns