Auxetic Photopolymer Structures: Geometry, Manufacturing Defects, Strain Range and Failure

Segurola, Juan

2026-10-03 · Report · Version 0.2

Auxetic response is a geometric mechanism that can be lost through small changes in hinge thickness, re-entrant angle, node shape or material nonlinearity. ER-362 focuses on the conditions under which a negative Poisson response remains measurable, repeatable and structurally useful after photopolymer manufacture. Full-field strain measurements are coupled to as-built geometry and local damage inspection so that kinematic rotation can be distinguished from hinge bending, fracture or out-of-plane buckling. Strain-range, orientation and defect perturbations establish the usable auxetic window. Qualification therefore requires not only a negative Poisson ratio, but retention of the intended deformation mode and an explicit limit on damage accumulation and manufacturing sensitivity.

ER-362.

© Juan Segurola.

All rights reserved

Full text

© Juan Segurola. Rights and exceptions. Specific Zenodo terms prevail.

Version DOI 10.5281/zenodo.23126836 · All versions in Zenodo

Related publications

Series overview: ER · Engineering Reviews

Previous publication: Mechanical Metamaterials Made by Photopolymerisation: Unit Cells, Boundary Effects, Nonlinearity and Qualification

Next publication: Functionally Graded Lattices in Photopolymer Additive Manufacturing: Gradient Definition, Interface Continuity and Performance